Ceramic Ink Dispersants (Super Dispersants): Stabilizing Water-Based Ink Systems

2026-09-18 17:09:28

Click:

Key Points of This Article

  • ›The application scope of ink dispersants (super dispersants): dispersion of polar fine inorganic pigments.
  • ›Four major advantages of water-based ink: can be cleaned directly with water, the system medium can be entirely water, inorganic pigments develop deeper and more vivid colors and dry faster, and steric hindrance prevents re-agglomeration and sedimentation.
  • ›Dispersion stability relies on two legs: electrostatic repulsion + steric hindrance. Organic pigments and inorganic pigments take different routes.
  • ›The key to suppressing 're-agglomeration' is the thickness of the adsorption layer — when the dispersant adsorption layer reaches sufficient thickness, the repulsive force between particles is enough to prevent flocculation.

The ink used in ceramic inkjet printing is essentially a suspension system with high solid content, ultrafine particle size, and long-term standing. It must remain stable in the print head without clogging, spread quickly into a film after ejection, and develop accurate color after firing. These three requirements are inherently contradictory, and the dispersant is the key auxiliary that balances them.

I. Why the Water-Based System Is Worth Switching To

The most direct benefit of switching from solvent-based to water-based is safety and environmental protection: water-based ink can be cleaned directly with water, is non-toxic and odorless, and is not flammable or explosive, reducing the safety management costs of the workshop and transportation.

The second is cost. The medium of the water-based ink system can be entirely water, resulting in lower costs for raw materials, production, and use. Hidden expenses such as solvent recovery and waste liquid treatment are also reduced accordingly.

The third is color development. The water-based system enables inorganic pigments to develop deeper and more vivid colors, dry faster, and avoid separation of glaze and ink — this is especially critical for products with high requirements for glaze surface effects.

II. Why Pigments 'Re-Agglomerate' and Settle

The inorganic pigments used in ceramic ink (such as zirconium-based, cobalt-based, and chrome-iron systems) have very small particle sizes after grinding, extremely large specific surface areas, and high surface energy. The system is thermodynamically unstable, and particles tend to approach each other to reduce surface energy. This process manifests as flocculation and agglomeration, which macroscopically appears as 're-agglomeration' and sedimentation.

Once re-agglomeration occurs, the consequences are chain-like: increased particle size raises the risk of clogging the inkjet channel; tinting strength and color strength decrease, requiring a larger ink volume to achieve the same color depth; the slurry stratifies in the ink storage tank, widening the color difference between batches.

Root Cause

Re-agglomeration is not 'not grinding finely enough,' but failing to stabilize the particles after grinding them fine. Grinding only solves the primary particle size problem; the dispersant solves the retention problem.

III. How Steric Hindrance Dispersion Works

There are two common routes for stabilizing ultrafine particles.

  • Electrostatic repulsion: The dispersant ionizes in water and is adsorbed on the pigment surface to form a charged layer. Particles repel each other due to like charges. This route is sensitive to electrolyte concentration, and Ca²⁺ and Mg²⁺ in the ink-making water compress the electric double layer and weaken the repulsive force.
  • Steric hindrance: One end of the dispersant's polymer chain segment is anchored to the pigment surface, while the other end extends into the medium, forming an adsorption layer with thickness. When two particles approach, the adsorption layers squeeze against each other and slide apart, physically blocking the particles from adsorbing each other.

The design concept of super dispersants is to superimpose these two routes: carrying both charge and a sufficiently long polymer solvation layer. When the adsorption layer thickness on the powder surface reaches the order of 8~9 nm, the repulsive force between particles is already sufficient to protect the system from flocculation. This is why polymer dispersants are usually superior to ordinary surfactants.

The water-based ink system prevents inorganic pigments from re-agglomerating and settling precisely through steric hindrance, thereby giving the product a longer shelf life.

IV. Four Conditions That Super Dispersants Must Meet

  1. 1Firm anchoring. The adsorption groups must be able to form sufficiently strong bonds with the polar inorganic pigment surface; otherwise, they will desorb during dilution, stirring, and temperature fluctuations.
  2. 2Sufficiently long solvated chains. The degree of chain segment extension in water determines the adsorption layer thickness, and thus the effectiveness of the steric barrier.
  3. 3Insensitivity to electrolytes. Ions introduced by the ink-making water and pigments are unavoidable, and the dispersant must not fail due to increased ionic strength.
  4. 4No impact on firing. Ceramic ink ultimately has to burn off organic matter, and the dispersant must completely decompose at the firing temperature, leaving no residue and not affecting color development.

V. Process Points from Grinding to Ink Formation

The effect of the dispersant is highly dependent on how it is used. The conventional practice is to adopt the order of 'wetting — grinding — stabilizing': first let the dispersant fully wet the pigment surface, then enter the grinding process to reduce particle size, and finally add a small amount of dispersant to stabilize the newly exposed surface.

If the order is reversed — grinding first and then adding the dispersant — the newly generated surface cannot be fully coated in time, and the probability of re-agglomeration increases significantly. This is a common reason why many on-site situations show 'the same formula and the same grinding conditions, but the effect is sometimes good and sometimes bad.'

Table 1 Troubleshooting Checklist for the Dispersion Stage of Water-Based Ceramic Ink

Stage of ConcernCommon ProblemAdjustment Direction
Timing of dispersant additionAdded after grinding, particles re-agglomerateAdd the dispersant before grinding so it fully wets the pigment
Ink-making water qualityHigh hardness and many ions weaken electrostatic repulsionControl water quality, prioritize relying on steric hindrance to stabilize the system
Cooling and temperature riseGrinding temperature rise causes desorptionControl grinding temperature, avoid prolonged high temperatures
Storage conditionsStanding stratification, bottom cakingRegularly circulate at low speed or roll to avoid long-term standing

VI. How to Measure the Effect

When evaluating the effect of a dispersant, it is recommended to look at four indicators at the same time: particle size distribution (especially the trends of D50 and D99), the stability of slurry viscosity over time, the standing stratification situation, and the color depth and color difference after firing. Measuring only the initial viscosity cannot reflect long-term stability.

The specific formula of the ink system falls within the customer's process scope. The company can provide super dispersant samples and dispersion solution recommendations, and work with customers to complete grinding and stability testing.

0
Ceramic Ink Dispersants (Super Dispersants): Stabilizing Water-Based Ink Systems
The ink used in ceramic inkjet printing is essentially a suspension system with high solid content, ultrafine particle size, and long-term standing. It must remain stable in the print head without clogging, spread quickly into a film after ejection
Long by picture save/share
CHASE 超速
 

Email: JEFF@CSCHEMICA.NET

Headquarters Address: Room 1806-1808, Building 36, Yiyun Xicheng, Keji North Road, Shishan Town, Nanhai District, Foshan City

Factory Address: Datianfeng Industrial Zone, Wuzhuang, Luocun, Shishan Town, Nanhai District, Foshan City

Hotline0757-82563626
二维码

© 2026 Foshan Chaoso Technology Co., Ltd.  All Rights Reserved   Yue ICP Bei No. 2020092827-1   Technical Support:Sheyu Technology

Add WeChat friend to learn more about the product
Use Enterprise WeChat
"Scan" to join the group chat
Copy success!
Add WeChat friend to learn more about the product
I see.