Ceramic Body Reinforcing Agent as a Replacement for CMC: The Double Account of Green Body Strength and Cost

2026-09-18 17:00:00

Click:

Key Points of This Article

  • ›The core value of the body reinforcing agent: improves the strength and toughness of the pressed green body, ensuring the tiles are not easily broken before entering the kiln.
  • ›In terms of flexural strength and price, it is superior to CMC (sodium carboxymethyl cellulose) and can fully replace it.
  • ›The dosage is very low: 0.1%~0.3% relative to the dry material, ultimately adjusted according to the actual condition of the soil sample.
  • ›Simple usage: add it together with the formula body mud, sand, and water into the ball mill, until the slurry is discharged, spray-dried, and pressed into shape.

Ceramic factories' requirements for green body strength often do not come from the performance of the final product, but from the pass rate of the production line. From the time the green tile leaves the press to entering the kiln, it passes through multiple stages such as conveyor belts, turning, stacking, and drying, and each transfer is a moment of stress. If the green body strength is insufficient, the damage rate goes up, the amount of recycled material increases, and both output and energy consumption are affected.

I. Why CMC Is Being Replaced

Sodium carboxymethyl cellulose (CMC) has long been used as a body reinforcing agent. Its mechanism is to form organic polymer bridges between particles, thereby increasing the mechanical strength of the green body. However, it has several unavoidable problems.

  • Both unit price and dosage are relatively high. To achieve the same flexural strength, the dosage of CMC is usually higher than that of a dedicated reinforcing agent, resulting in higher overall auxiliary costs.
  • Impact on slurry rheology. The thickening effect of the polymer raises slurry viscosity and somewhat counteracts the effect of the deflocculant, requiring additional balancing in the formula.
  • Many concerns about batch stability. The degree of substitution and molecular weight distribution of CMC affect the reinforcing effect, and fluctuations are more obvious when purchasing from multiple sources.

Dedicated body reinforcing agents take a different route: they form effective inter-particle bonding at a small dosage, while improving flexural strength and toughness more directly, so they can 'fully replace CMC' while improving both strength and cost at the same time.

II. Two Forms, How to Choose

Table 1 Specification Comparison Between Powdered and Liquid Body Reinforcing Agents

ItemBody Reinforcing Agent (Powdered)Liquid Reinforcing Agent
AppearanceWhite powderWhite or light yellow liquid
Packaging Specifications25±0.25 kg, inner plastic bag with outer woven bag25 kg plastic drum
Application ScopeFloor tiles, wall tiles, daily-use ceramics, sanitary ceramics, etc.Floor tiles, wall tiles, daily-use ceramics, sanitary ceramics, etc.
PerformanceIncreases green body strength and toughness, can fully replace CMC, flexural strength and price significantly better than CMCIncreases green body strength and toughness, can fully replace CMC, flexural strength enhancement and price significantly better than CMC
Dosage0.1%~0.3% relative to dry material0.1%~0.3% relative to dry mud
UsageAdd together with body mud, sand, and water into the ball millAdd together with body mud, sand, and water into the ball mill
StorageNon-toxic and non-corrosive, shelf life of 24 months in a dry environmentNon-toxic and non-corrosive, shelf life of 24 months in a dry environment

The choice is mainly based on the material form and degree of automation of the production line: production lines that already have liquid metering and piping work more smoothly with liquid products, while pure powder batching lines can implement powdered products faster. There is no essential difference between the two in terms of target performance.

III. The Logic Behind 0.1%~0.3%

The dosage of the reinforcing agent is only 0.1%~0.3% relative to the dry material, which seems very small, but this range is already sufficient to cover most body materials. Why can't you simply copy someone else's value? Because the reinforcing effect depends on three variables: soil particle size distribution, powder moisture content, and pressing pressure.

  1. 1Particle size distribution. For body materials with tight grading and little fine powder, there are more contact points between particles, and the green body strength itself is higher, so the reinforcing agent dosage can be taken at the lower limit.
  2. 2Powder moisture content. When the moisture of the powder coming out of spray drying is on the high side, there is more bound water between particles, and the effect of the reinforcing agent is more easily reflected. If the moisture is too low, the dosage needs to be slightly increased.
  3. 3Pressing pressure. The higher the pressure and the higher the green body density, the lower the marginal contribution of the reinforcing agent, and at this point the dosage should not be blindly increased.
  4. 4Soil sample batch. After changing the mining site, it needs to be reconfirmed. The product data also clearly states that 'ultimately it is adjusted according to the actual condition of the soil sample.'

IV. Usage and Feeding Timing

The usage is not complicated: add the reinforcing agent together with the formula body mud, sand, and water into the ball mill, until the slurry is discharged, spray-dried, and pressed into shape. The key is to disperse the reinforcing agent evenly. If the local concentration is too high, local unevenness in body strength will occur, which instead becomes a starting point for cracking. For powdered products, it is recommended to pre-mix with a small amount of dry material before feeding, while liquid products can be metered directly into the ball mill inlet.

Important Reminder

Adding the reinforcing agent into the ball mill means 'grinding together,' not 'adding after grinding.' Adding after grinding makes it difficult to achieve uniform dispersion, and the reinforcing effect will be discounted.

V. How to Verify the Effect

The testing method recommended in the company's product data is very practical: add a certain amount of reinforcing agent to a small ball milling jar containing formula body mud and sand, then after grinding, press small bricks to compare their flexural strength.

  1. 1Prepare control groups. One group without reinforcing agent, one group with CMC (at the current dosage), and one group with reinforcing agent (at three levels: 0.1%, 0.2%, and 0.3%).
  2. 2Unify sample preparation conditions. Ball milling time, slurry moisture content, pressing pressure, and holding time must be consistent; otherwise, the flexural strength is not comparable.
  3. 3Measure flexural strength. Use the same instrument to test small brick test bars of the same size, and record the average value and dispersion. The dispersion itself is also an indicator of dispersion uniformity.
  4. 4Calculate the overall cost. Do not just compare unit prices; compare the 'auxiliary cost per unit of dry material' — that is, the unit price multiplied by the dosage required to reach the target strength.

VI. How to Calculate the Cost Account Accurately

The account for replacing CMC is usually reflected in three places: first, the unit cost of the auxiliary itself; second, the change in deflocculant dosage after the slurry rheology improves; and third, the reduction in recycled material and the increase in output brought about by the decrease in green body damage rate. The second and third items are often larger than the first, but are most easily overlooked during the evaluation stage.

The recommended practice in practice is: first conduct a two-week comparison on one production line, recording auxiliary costs, slurry parameters, pressing parameters, green body damage rate, and firing pass rate, and then make a full switch decision. Data is more convincing than unit price.

0
Ceramic Body Reinforcing Agent as a Replacement for CMC: The Double Account of Green Body Strength and Cost
The core value of the body reinforcing agent: improves the strength and toughness of the pressed green body, ensuring the tiles are not easily broken before entering the kiln. ›In terms of flexural strength and price, it is superior to CMC (sodium carboxymethyl cellulose) and can fully replace it. ›The dosage is very low: 0.1%~0.3% relative to the dry material, ultimately adjusted according to the actual condition of the soil sample. ›Simple usage: add it together with the formula body mud, sand
Long by picture save/share
CHASE 超速
 

Email: JEFF@CSCHEMICA.NET

Headquarters Address: Room 1806-1808, Building 36, Yiyun Xicheng, Keji North Road, Shishan Town, Nanhai District, Foshan City

Factory Address: Datianfeng Industrial Zone, Wuzhuang, Luocun, Shishan Town, Nanhai District, Foshan City

Hotline0757-82563626
二维码

© 2026 Foshan Chaoso Technology Co., Ltd.  All Rights Reserved   Yue ICP Bei No. 2020092827-1   Technical Support:Sheyu Technology

Add WeChat friend to learn more about the product
Use Enterprise WeChat
"Scan" to join the group chat
Copy success!
Add WeChat friend to learn more about the product
I see.